Classifications: AWS/SFA 5.1 E7018       IS 814 EB
5426H3JX
Description: A heavy coated, low hydrogen, iron powder type
electrode producing tough
and ductile weld metal .It has pleasing operating characteristics. Operating in
all positions depositing X-rays quality welds. Specially recommended for
heavy joints under restrain and those subject to dynamic loading. Deposition
efficiency is 115% approx.
Applications:
- Heavy structure.
- Boilers.
- Pressure vessels.
- Penstocks.
- Earth
moving equipments.
- Railways coaches wagons & locomotives.
- Pipe
lines.
Weld Metal Chemistry (%):
| C |
Mn |
Si |
S |
P |
| 0.10 max |
0.80 - 1.40 |
0.60 max |
0.03 max |
0.03 max |
All Weld Mechanical Properties:
| UTS (N/mm2) |
YS (N/mm2) |
Elongation (%) (L=4xD) |
CVN Impact values |
At temp. |
| 510-600 |
450-540 |
22-30 |
50-80 J |
-30°C |
Welding Currents: (Amp)
| 2.5 mm |
3.15 mm |
4.0 mm |
5.0 mm |
| 70-100 |
100-140 |
140-180 |
190-230 |
Diffusible H2 Content, ml 100 gm < 5