Used for fabrication of Light metal structures, General purpose fabrication, automobile bodies,steel furniture, railway coaches & wagons, Pipe, grills, storage tanks, construction lines, bridges etc., even at low current.
| C | Mn | Si | S | P |
|---|---|---|---|---|
| 0.10 max | 0.35 - 0.50 | 0.30 max | 0.03 max | 0.03 max |
| C | YS (N/mm2) | Elongation (%) (L=4xD) | CVN Impact values | At temp. |
|---|---|---|---|---|
| 410-540 | 360-440 | 22-26 | 50-80 J | 0°C |
| 2.5 mm | 3.15 mm | 4.0 mm | 5.0 mm |
|---|---|---|---|
| 60-80 | 90-130 | 140-180 | 180-230 |
| C | Mn | Si | S | P |
|---|---|---|---|---|
| 0.10 max | 0.40 - 0.50 | 0.30 max | 0.03 max | 0.03 max |
| UTS (N/mm2) | YS (N/mm2) | Elongation (%) (L=4xD) | CVN Impact values | At temp. |
|---|---|---|---|---|
| 430-540 | 360-440 | 22-30 | 50-70 J | 0°C |
| 2.5 mm | 3.15 mm | 4.0 mm | 5.0 mm |
|---|---|---|---|
| 60-80 | 90-130 | 140-180 | 190-230 |
| C | Mn | Si | S | P |
|---|---|---|---|---|
| 0.10 max | 0.40 - 0.60 | 0.30 max | 0.03 max | 0.03 max |
| UTS (N/mm2) | YS (N/mm2) | Elongation (%) (L=4xD) | CVN Impact values | At temp. |
|---|---|---|---|---|
| 440-550 | 380-440 | 22-30 | 50-75 J | 0°C |
| 2.5 mm | 3.15 mm | 4.0 mm | 5.0 mm |
|---|---|---|---|
| 60-80 | 90-130 | 140-180 | 190-230 |