Classifications:ASME SECTION || PART C SFA 5.18-ER 70S.6
FEATURES:
- Smooth Feeding.
- Perfect Layer Winding in all Sizes.
- Controlled Cast and Helix.
- Smooth Current Pick-up.
- Minimum Contact Tip Wear.
- Stable Arc and Minimum Spatter.
Industries:
- Automotive .
- Industrial and General Fabrication.
- Ship Building
.
- Trailers, Earth Moving Equipment
.
- Railway Wagon, Storage Tanks
.
Weld Metal Chemistry (%):
| C |
Mn |
Si |
S |
P |
| 0.06-0.15 |
1.40-1.85 |
0.80-1.15 |
0.035 max |
0.025 max |
| Cr |
Ni |
V |
Mo |
Cu |
| 0.15 max |
0.15 max |
0.03 max |
0.15 max |
0.50 max |
All Weld Mechanical Properties:
| U.T.S |
YS (N/mm2) |
Elongation (%) (L=4xD) |
CVN Impact 29° C |
| 510 |
424 |
22 |
27J |
Welding Currents: (Amp)
| SIZE (mm) |
Current (Amps) |
In Amps |
In Volts |
Gas Flow L/M |
| 0.8 |
DC [+] |
50-180 |
18-25 |
10-25 |
| 1.0 |
DC [+] |
80-200 |
20-26 |
12-20 |
| 1.2 |
DC [+] |
130-300 |
22-36 |
16-28 |
| 1.6 |
DC [+] |
200-400 |
24-38 |
16-28 |